Effect of delaying addition time of SMF superplasticizer on the physic-mechanical properties and durability of cement pastes
• 2012
Publication Information
Authors
H. El-Didamony, Mohamed Heikal, Kh.A. Khalil, S. Al-Masry
Keywords
Not Available
Journal
Not Available
Publisher
Not Available
Volume
Not Available
Issue
Not Available
Pages
Not Available
publication.type
International
Paper Link
Open Link
Supplementary Materials
Not Available
Abstract
This research aimed to investigate the influence of delaying addition time of laboratory prepared sulphonate melamine formaldehyde (SMF) superplasticizer on the physico-mechanical characteristics and durability of cement pastes subjected to elevated temperature up to 800 °C, or immersed in 4% MgSO4 and 4% MgCl2. The compressive strength increases with delayed addition time at 7.5 min up to 90 days. The cement pastes containing 1.0 mass% SMF superplasticizer, with delayed addition time at 7.5 min, has highest compressive strength, bulk density and lower total porosity. The presence of SMF superplasticizer with delaying addition time process of mixing increases the compressive strength, bulk density and decreases the total porosity. These work together to produce a compact structure, inhibiting the chloride and sulphate ions penetration, hence the total sulphate and chloride contents decrease.
Staff Members - Benha University