Study on the movement of wire electrode during fine wire electrical discharge machining process
Journal of Materials Processing Technology • 2016
معلومات البحث
المؤلفون
Sameh Habib; Akira Okada
الكلمات المفتاحية
Wire EDM
Tungsten wire
High-speed observation
Wire movement
Wire deflection
Amplitude envelope
المجلة العلمية
Journal of Materials Processing Technology
الناشر
Elsevier
المجلد
227
العدد
Not Available
الصفحات
147-152
publication.type
International
رابط البحث
Not Available
المواد المرفقة
Not Available
الملخص
Wire movements and vibrations are one of the most important phenomena of wire electrical discharge
machining (EDM) process. Unstable wire electrode behavior and large wire vibration amplitude during
the process cause wire breakage, low shape accuracy and large machined surface roughness. In this study,
direct observation using high-speed camera investigated the movements of tungsten wire electrode
during fine wire EDM process. The results showed that the vibration amplitude and frequency depended
mainly on the wire tension, and the amplitude direction. The amplitude in the direction parallel to the
machining direction was a little larger than that in the perpendicular one. In addition, the backward
deflection of wire could be confirmed even in fine wire EDM. Also, the wire vibration mode was analyzed,
and it could be varied with the machining position of the thin workpiece, which possibly led to smaller
wire amplitude. Furthermore the amplitude envelope of wire electrode during the process was clarified
machining (EDM) process. Unstable wire electrode behavior and large wire vibration amplitude during
the process cause wire breakage, low shape accuracy and large machined surface roughness. In this study,
direct observation using high-speed camera investigated the movements of tungsten wire electrode
during fine wire EDM process. The results showed that the vibration amplitude and frequency depended
mainly on the wire tension, and the amplitude direction. The amplitude in the direction parallel to the
machining direction was a little larger than that in the perpendicular one. In addition, the backward
deflection of wire could be confirmed even in fine wire EDM. Also, the wire vibration mode was analyzed,
and it could be varied with the machining position of the thin workpiece, which possibly led to smaller
wire amplitude. Furthermore the amplitude envelope of wire electrode during the process was clarified