Effect of organic acids precursors on the morphology and size of ZrO2 nanoparticles for photocatalytic degradation of Orange G dye from aqueous solutions
Journal of Molecular Liquids • 2016
معلومات البحث
المؤلفون
Islam M. Ibrahim⁎, Moustafa E. Moustafa, Mohamed R. Abdelhamid
Chemistry Department, Faculty of Science, Benha University, 13518, Egypt
الكلمات المفتاحية
Keywords:
Zirconium oxide nanoparticles
XRD
HR-TEM
Photocatalytic degradation
Orange G dye
المجلة العلمية
Journal of Molecular Liquids
الناشر
Elsevier
المجلد
Journal of Molecular Liquids 223 (2016) 741–748
العدد
Journal of Molecular Liquids 223 (2016) 741–748
الصفحات
741-748
publication.type
International
رابط البحث
Not Available
المواد المرفقة
Not Available
الملخص
Zirconium oxide nanoparticles were prepared by precipitation from different organic acid precursors (oxalic,
tartaric, citric, succinic, malic, maleic and malonic) and ignition at 750 °C. The as-prepared samples were characterized
by XRD, FT-IR, UV–Vis and HR-TEM techniques. XRD proved the crystalline monoclinic structure of the
samples with average crystal sizes ranged from 7.1 nm (for citrate) to 35.1 nm (for maleic) precursor. The FTIR
spectra of the nanooxides showed the characteristic bands due to νOH, δOH and νZr-O at 3444, 1633 and
498 cm−1, respectively. The UV–Vis spectra proved the semiconductor nature of the samples with optical energy
gap ranging from 1.80 to 4.30 eV. One of the prepared sampleswas tested as catalyst for the photodegradation of
Orange G dye in wastewater samples in presence of H2O2 where 100% removal of the dye was obtained after
about 180 min.
tartaric, citric, succinic, malic, maleic and malonic) and ignition at 750 °C. The as-prepared samples were characterized
by XRD, FT-IR, UV–Vis and HR-TEM techniques. XRD proved the crystalline monoclinic structure of the
samples with average crystal sizes ranged from 7.1 nm (for citrate) to 35.1 nm (for maleic) precursor. The FTIR
spectra of the nanooxides showed the characteristic bands due to νOH, δOH and νZr-O at 3444, 1633 and
498 cm−1, respectively. The UV–Vis spectra proved the semiconductor nature of the samples with optical energy
gap ranging from 1.80 to 4.30 eV. One of the prepared sampleswas tested as catalyst for the photodegradation of
Orange G dye in wastewater samples in presence of H2O2 where 100% removal of the dye was obtained after
about 180 min.