Banner

Mechanical, Microstructure & Tribological Properties of PM Al-25%Si/Al2O3 Composites

First Afro-Asian Conference on Advanced Materials Science and Technology • 2006
العودة
معلومات البحث
المؤلفون S. F. Moustafa, A. M. Gaafer. , A. Alakabawy , M. I. Algzzar ,
الكلمات المفتاحية PM, Al-25Si, Composites, Al2O3
المجلة العلمية First Afro-Asian Conference on Advanced Materials Science and Technology
الناشر First Afro-Asian Conference on Advanced Materials Science and Technology
المجلد Not Available
العدد Not Available
الصفحات Not Available
publication.type International
رابط البحث Not Available
المواد المرفقة Not Available
الملخص
The processing of Al-25%Si alloy reinforced by 0, 5, 10 and 15wt. % Al2O3 using PM technique by mixing of powder in a double cone mixer, warm compaction of composite powder followed by sintering at temperature of 550ã C for one hour. The mechanical properties, microstructure features, electrical resistivity and wear rate were measured. The results show that the powder of (Al-25%Si) produced by atomization is almost spherical in shape with average particle size of
150µm, apparent density of 0.949g/cm3 and flow rate of 22 s / 50gm. Optical investigation of sintered specimens shows a fairly good distribution of reinforced alumina particles through out the microstructure. Compressive strength increases by adding Al2O3 reinforcement but exhibits a
low ductility. Hardness value increases directly by the increase of reinforcement percent.
Composites containing 15% Al2O3 exhibits a high hardness (152 Hv) and excellent wear resistance.